Ruby
The red variety of corundum, colored by chromium, second only to diamond in hardness among the common gems.

Technical data
- Mineral species and variety
- Corundum, red variety
- Chemical composition
- Al2O3 (aluminium oxide) with chromium
- Crystal system
- Trigonal
- Mohs hardness
- 9
- Refractive index
- 1.762–1.770
- Specific gravity
- 3.95–4.10
- Toughness and cleavage
- Toughness is good and there is no true cleavage, but corundum can part along twinning planes, and fissures weaken a stone.
- Color and cause of color
- Pinkish red to purplish red and pure red; chromium causes the red, and iron can darken or brown the color.
Treatments and disclosure
- Most rubies are heated to improve color and clarity; this is stable and widely accepted.
- Heating with fluxes can heal fissures and leave glassy residues inside them.
- Lead-glass filling of heavily fractured material produces a composite ruby that is much less durable.
- Dyeing and oiling of surface-reaching fissures are also seen in low-grade material.
Treatments must be disclosed under the FTC Jewelry Guides when they are not permanent, need special care or significantly affect value. Lead-glass filling must always be disclosed, with its special care; laboratories describe these stones as filled or composite material.
Lab-created and imitation counterparts
- Laboratory-created ruby is grown by flame fusion, flux or hydrothermal methods and must be described as laboratory-created or synthetic.
- Red glass, garnet-and-glass doublets and red spinel have been used as imitations or confused with ruby.
Ask for a laboratory report when the treatment status affects the value of the piece.
Cutting and sizes
Ovals and cushions are the most common shapes for center stones, followed by rounds, pears and emerald cuts. Cabochons are used for star ruby and translucent material.
Calibrated rounds, ovals, squares and baguettes are standard for accents and line work, for example 3 mm rounds or 5 × 3 mm, 6 × 4 mm and 7 × 5 mm ovals. Larger stones are matched individually.
Setting and bench notes
Prong, bezel, halo, channel and pavé settings all suit ruby.
- Heat at the torch
- Remove the stone before torch work unless it is confirmed unheated or heat-only, and even then protect it and let it cool slowly. Never heat a glass-filled ruby or put it in pickle.
- Ultrasonic and steam cleaning
- Ultrasonic and steam cleaning are usually safe for untreated or heat-only stones. Avoid both for glass-filled, fracture-filled or dyed stones.
- Pressure when setting
- Ruby takes normal setting pressure well; take care over open fissures and thin culets.
Durability and care
- Rings
- Very good for daily-wear rings when the stone is untreated or heat-only.
- Earrings and pendants
- Very good in earrings and pendants; glass-filled stones are better kept to these lower-wear pieces.
Care
- Clean with warm water, mild soap and a soft brush.
- Keep glass-filled rubies away from acids, including lemon juice, and from jewelry cleaning solutions.
Sources and lab reports
Principal commercial sources include Myanmar, Mozambique, Madagascar, Tanzania, Thailand, Sri Lanka and Vietnam. Some markets restrict gems from certain origins, so ask for origin documentation where yours requires it.
GIA, SSEF, Gübelin, AGL and Lotus Gemology reports are commonly requested for important stones, often with an origin opinion and a statement of heating.
JewelsRova manufactures the jewelry. Stones are sourced through our vetted suppliers and named on the quotation, with any treatment disclosed.
Laboratory reports are available on request.
Minimums start at 1 piece for bespoke fine jewelry, 5 pieces per design in solid gold and 20 pieces per design in 925 silver or vermeil.
Questions buyers ask
Is heated ruby acceptable in fine jewelry?
Yes. Heating is long-established, stable and accepted by the trade, but it should be disclosed. Unheated ruby with a report is a separate, higher category.
What is a glass-filled ruby?
Heavily fractured corundum filled with lead glass. It looks like ruby but is far less durable, can be damaged by heat and acids, and must be disclosed as filled or composite material.
What is the difference between ruby and pink sapphire?
Both are corundum. The line between red ruby and pink sapphire is a judgment of color saturation, and laboratories and markets can draw it differently.